高流动/易加工/PA66/美国杜邦/101F/杜邦尼龙 杜邦PA标准产品
产品参数
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |||
基本性能 | 吸水率 | 24hr | ASTM D-570 |
|
% | ||
密度 | ASTM D-792 |
|
g/cm3 | ||||
物理性能 | 阻燃性 | UL 94 |
|
mm | |||
比重 | ASTM D-792 |
|
|||||
模具收缩率 |
|
% | |||||
机械性能 | 拉伸强度 | ASTM D-638 |
|
MPa | |||
断裂拉伸强度 | ASTM D-638 |
|
MPa | ||||
断裂伸长率 | ASTM D-638 |
|
% | ||||
弯曲模量 | ASTM D-790 |
|
MPa | ||||
屈服伸长率 | ASTM D-638 |
|
% | ||||
IZOD缺口冲击强度 | ASTM D-256 |
|
J/m | ||||
电气性能 | 介电强度 | 3.2mm | ASTM D-149 |
|
kv/mm | ||
体积电阻率 | ASTM D-257 |
|
Ω.cm | ||||
介电常数 | 103Hz | ASTM D-150 |
|
||||
损耗因数 | 103Hz | ASTM D-150 |
|
||||
介电常数 | 106Hz | ASTM D-150 |
|
||||
损耗因数 | 106Hz | ASTM D-150 |
|
||||
损耗因数 | 102Hz | ASTM D-150 |
|
||||
表面电阻率 | ASTM D-257 |
|
Ω | ||||
介电强度 | 1.6mm | ASTM D-150 |
|
kv/mm | |||
热性能 | 热变形温度 | 1.80MPa | ASTM D-648 |
|
℃ | ||
熔点 | ASTM D-3418 |
|
℃ | ||||
热变形温度 | 0.45MPa | ASTM D-648 |
|
℃ |